Magnesite Brick — 91%
The same basic brick at approximately 91% MgO. The extra magnesia displaces silicate bonding phase between the grains, which is where the low-melting compounds form — so the gain over the 90% grade is chemical resistance at the grain boundaries, not a higher temperature rating.

| Shape | Rectangle |
|---|---|
| Application | Side Walls, Partition Walls, Roof |
| Resistance Durability | Heat Resistant |
Values as published by the manufacturer. Manufacturer TDS governs.
Steelmaking furnace and rotary kiln linings, glass furnace regenerators, and hearth and soaking-zone duty where the 90% grade is being consumed faster than the campaign allows. Same hydration caution: store dry.
Read the engineering note →Manufacturer technical datasheets and safety data sheets for this line are available on request — ask for them with your enquiry and we will send them with the quotation.
Request the datasheet →More in Bricks
Bricks
Magnesite Brick — 90%
Bricks
High Alumina Fire Brick — 30%
Bricks
High Alumina Fire Brick — 40%
Bricks
High Alumina Fire Brick — 50%
Bricks
High Alumina Fire Brick — 60%
Bricks
High Alumina Fire Brick — 70%
Bricks
High Alumina Fire Brick — 80%
Bricks
Acid Resistant Brick
Bricks
HFK Insulation Brick
Bricks
INS 110
Bricks
INS 140
Bricks
Porosint 500
Bricks
Porosint 750
Bricks
Alumina Burner Block
Bricks
Refractory Fire Tile