INSULYTE 7

0.72 g/cc dried at 1100 °C service, with thermal conductivity of 0.14 kcal/m/hr/°C at 800 °C hot face and 6.0 kg/cm² cold crushing strength. Iron oxide is 9.8%. A backup insulating grade — light, weak, and low in conductivity by design.

INSULYTE 7 — product visual
Representative product visual
Technical specifications for INSULYTE 7
NATURE OF BONDHYDRAULIC
Maximum Service Temperature1100°C
Maximum grain size6 mm
Fe₂O₃ content, %9.8
Dry density, g / cc0.72
Cold crushing strength, kg/cm²6.0
PLC, % after heating at 1250 ºC / 24 hrs-0.35
Thermal Conductivity Kcal/m/hr/ºC at 800ºC HF0.14
Packaging25 kg bags
Storage Life9 months

Values as published by the manufacturer. Manufacturer TDS governs.